| 缓解铅酸蓄电池正极活性物质脱落的措施 |
| Measures to Slow Exfoliation of Active Matter from Positive Pole of a Sulphuric Accumulator |
| |
| DOI: |
| 中文关键词: 铅蓄电池 正极板 活性物质 措施 |
| 英文关键词: plumbous acid accumulator positive plate active matter measures |
| 基金项目: |
|
| 摘要点击次数: 6608 |
| 全文下载次数: 5557 |
| 中文摘要: |
| 分析了放电温度、放电电流及硫酸浓度等因素对铅蓄电池正极活性物质脱落的影响,并提出了相应的措施. |
| 英文摘要: |
| The author analyses the influence of discharge temperature, discharge current anddensity of sulphric acid on exfoliation of active rnatter from the positive pole of a plumbousacid accumulator, and puts forward some corresponding measures. |
|