文章摘要
粉煤灰增强树脂基摩擦材料的热处理工艺研究
Research on Heat Treatment Process of Resin-based Friction Material Filled with Fly Ash
  
DOI:10.3969/j.issn.1671-5322.2010.04.007
中文关键词: 粉煤灰  树脂基摩擦材料  摩擦磨损  热处理
英文关键词: fly ash  resin-based friction material  friction and wear  heat treatment
基金项目:江苏高校自然科学重大基础研究项目,江苏省生态环境材料重点实验室开放基金资助项目
作者单位
王占红 盐城工学院江苏省生态环境材料重点建设实验室江苏盐城224051 
侯贵华 盐城工学院江苏省生态环境材料重点建设实验室江苏盐城224051 
朱祥 盐城工学院江苏省生态环境材料重点建设实验室江苏盐城224051 
摘要点击次数: 4534
全文下载次数: 3890
中文摘要:
      为了改进粉煤灰增强树脂基摩擦材料的摩擦学性能和制造工艺,对摩擦制动材料的热处理工艺参数:热处理温度和热处理时间分别进行了研究.实验结果表明:热处理温度为200 ℃,热处理时间10 h,制备的粉煤灰增强树脂基摩擦材料具有良好的力学性能和摩擦磨损性能.
英文摘要:
      Two heat treatment process parameters: heat treatment temperature and heat treatment time were studied for resin-based on friction materials containing fly ash in order to improve the tribology performance and forming techniques.It is indicated by experimentation that much better properties of friction and wear are achieved for resin-based on friction materials added fly ash on the condition of the heat treatment temperature 200 ℃,the heat treatment time 10 hours.